Sign In | Join Free | My insurersguide.com
China Eternal Bliss Alloy Casting & Forging Co.,LTD. logo
Eternal Bliss Alloy Casting & Forging Co.,LTD.
EB Castings&Forgings, Your Total Solution!
Verified Supplier

8 Years

Home > Cobalt Alloy Castings >

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

Eternal Bliss Alloy Casting & Forging Co.,LTD.
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

Brand Name : Eternal Bliss

Model Number : EB26078

Certification : ISO9001-2008

Place of Origin : China

MOQ : 30 kg

Price : USD80/kg ~ USD120/kg

Payment Terms : by T/T or L/C, Western Union

Supply Ability : 100,000,000.00

Delivery Time : It depends on the quantity to be ordered.

Packaging Details : Pallets

Material Grade : cobalt alloy 1, cobalt alloy 3,

Hardness Temperature : Up to 1200 Centi-degree

Coating Process : SPF Coating,overlay process

Cast Process : Wax Lost Process

Surface Treatment : Shot Blast

Contact Now

Precision Cast Process X-40 Cobalt High Speed Steel Products with High Accuracy EB26078

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products.

Precision investment casting services for a variety of high temperature super alloys cobalt-based types.

Provides on-site engineering support, tooling design, surface treatment, laboratory testing, and warehousing services. Just in time delivery and other logistics services are available.

We produce High Temperature Superalloy Castings Parts with precision investment process.

Table 1 : Standard Cobalt cobalt alloy Alloy

Co Cr C W Mo Ni Si B Fe Mn Others
cobalt alloy 1 BAL 33 2.45 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 3 BAL 31 2.5 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 4 BAL 31.5 1 14 - 2.0* 1 - 2.0* 1 -
BAL 28 1.2 5 - 3.0* 1 - 2.5* 1 -
cobalt alloy 12 BAL 29 1.85 9 - 2.5* 1 - 2.5* 1 -
cobalt alloy 20 BAL 33 2.45 17.5 - 2.5* 1 - 2.5* 1 -
cobalt alloy 21 BAL 27 0.25 - 5.5 2.5* 1 - 3.0* 1 -
cobalt alloy 31 BAL 26 0.5 7.5 - 10.5 1 - 2.0* 1 -
cobalt alloy 190 BAL 26 3.3 14 - 1.0 1 - 8.0 0.5 -
cobalt alloy 238 BAL 26 0.1 - 3 - 1 - 20.0 1 -
cobalt alloy 306 BAL 25 0.4 2 - 6.0 1 - 4.0* 1 Nb=5
94 BAL 28 1 19 - 5.0 1 - 2.5* 1 V=1
cobalt alloy F BAL 25.5 1.75 12.25 - 22.5 1 - 1.5* - -
cobalt alloy SF1 BAL 19 1.3 13 - 13 3 2.5 3* 0.5 Cu=0.5
cobalt alloy SF6 BAL 19 0.7 7 - 13 2.5 1.7 3* 0.5 Cu=0.5
cobalt alloy SF12 BAL 19 1 9 - 13 3 2 3* 0.5 Cu=0.5
cobalt alloy SF20 BAL 19 1.5 15 - 13 3 3 2* 0.5 Cu=0.5
TRIBALOY T400 BAL 8 0.1* - 28 3* 2.4 - 3* - -
TRIBALOY T800 BAL 17 0.1* - 28 3* 3.2 - 3* - -
DELORO 15 - - 0.06* - - BAL 2.0 1.05 1.5* 20 Cu=20
DELORO 22 - 0.70 0.10 - - BAL 2.3 1.75 - - -
DELORO 40 - 7.0 0.10 - - BAL 3.5 2.25 - - -
DELORO 50 - 10.25 0.45 - - BAL 4.0 1.85 4.0 - -
DELORO 60 - 14.25 0.6 - - BAL 2.0 3.5 4.0 - -
DELORO 625 - 22 0.1 - 9 BAL - - 5 - -
NISTELLE C - 16.5 0.12* 4.5 17 BAL 0.7 - 6.0 - -
TRIBALOY T700 - 15 0.10* - 32 BAL 3.25 -
Hastelloy C22®(UNS N06022)(Max.)
C MN P S Si Cr Ni Mo CO Fe W V
0.015 0.5 0.02 0.02 0.08 20.0-22.5 Bal. 12.5-14.5 2.5 2.0-6.0 2.5-3.5 0.35
Hastelloy C276®(UNS N10276)(Max.)
C MN P S Si Cr Ni Mo CO Fe W V
0.01 1 0.04 0.03 0.08 14.5-16.5 Bal. 15.0-17.0 2.5 4.0-7.0 3.0-4.5 0.35
Hastelloyx®(UNS N06002)(Max.)
C MN P S Si Cr Ni Mo CO Fe W other
0.05-0.15 1 0.04 0.03 1 20.5-23.0 Bal. 8.0-10.0 0.5-2.5 17.0-20.0 0.2-1.0 /
Monel 400®(UNS NO4400) (Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
C MN S Si Ni Cu Fe
0.3 2 0.024 0.5 63 min 28-34 2.5
Monel M400®(UNS NO4400)(Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
C MN S Si Ni Cu Fe
0.3 2 0.024 0.5 63-70 28-34 2.5
Monel R405®(UNS NO4405)(Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
C MN S Si Ni Cu Fe
0.3 2 0.025-0.06 0.5 63.0min 28-34 2.5
Monel K500®(UNS NO5500)(Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
C MN S Si Ni Cu Ti AI Fe
0.1 2 0.01 0.5 63min 27-33 0.86 2.3-3.15 2
Inconel 600(UNS NO6600)(Max.)
C MN S Si Cr Ni Cu Fe
0.15 1 0.015 0.5 14-17 72 min 0.5 6.0-10.0
Inconel 601(UNS NO6601)(Max.)
C MN Si Cr Ni CO AI Fe
0.05 0.3 0.2 22.5 61.5min 5 1.4 14.1
Inconel 718(UNS NO7718)(Max.)
Cr Ni Mo CO Cb+Ta Ti AI Fe
19 52.5min 3.05 5 5.13 0.9 0.5 18.5
Chemical Analysis of Incoloy 800® uns(N08800)
C Cr Ni Ti AI Fe Grain
0.1 max 19.0-23.0 30.0-35.0 0.15-0.6 0.15-0.6 39.5min /
Incoloy800H® UNS(N08810)
C Cr Ni Ti AI Fe Grain
0.05-0.1 19.0-23.0 30.0-35.0 0.15-0.60 0.15-0.60 39.5min 5or coarser
Incoloy800HT® UNS(N08811)
C Cr Ni Ti AI Fe Grain
0.06-0.10 19.0-23.0 30.0-35.0 0.25-0.60 0.25-0.60 39.5min 5or coarser

Dimensions:as per drawings

Production Process

Step 1: Getting orders.

Step 2: Process design by technical department

Step 3: Purchase of raw materials and pattern making &checking

Step 4: Inspection of raw materials

Step 5: Melting by middle-frequency induction furnaces

Step 6: Ladle analysis by Spectrometer

Step 7: De-oxidization, slag-removal, tapping

Step 8: Pouring

Step 9: Openning & fettling

Step 10: Surface & dimensional check

Step 11: Heat treatment

Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)

Step 13: Packing

Step 14: Shipping

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

1. 16-year Foundry Operation Experience.

2. Friendly & High Efficient Technical & Commercial Communication.

3. Professional Export Practices: Have Exported to +60 Overseas Countries.

Our Trade Show Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

Our booth No. 14-A29-5 in Newcast 2015,Germany

Hall 14, Stand No.A29-5.

Contact Us for further information about products & service:

Mr.John Liu

Project Manager

Cell: 0086-130 930 23772(What's App)

Tel: 0086-188 0059 6372

Fax: 0086-510-6879 2172

E-mail: cast@ebcasting.com; ebcastings@163.com

Skype ID:julia.zhu26

QQ: 217 039 6403

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Productswww.ebcastings.com


Eternal Bliss Alloy Casting & Forging Co.,LTD.

Product Tags:

precision steel casting

      

cast cobalt alloys

      
Cheap Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products for sale

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Eternal Bliss Alloy Casting & Forging Co.,LTD.
*Subject:
*Message:
Characters Remaining: (0/3000)